Torque-Force Graph Determination of the torque-tension relationship for a threaded fastener allowing the appropriate tightening torque to be determined. Such tests will allow the nut factor (sometimes referred to as the torque coefficient or k factor) to be determined. and the overall coefficient of friction. By completing several similar tests, the variation in the torque-tension relationship, due to friction variation, can be established for an application.